Arcaloy 309L-16 is used for welding carbon and low alloy steels to stainless steels. This can be done provided the service temperature does not exceed about 700°F (370°C). Post weld heat treatment should only be performed after due consideration.
Industries
- Industrial and General Fabrication
Welding Process
Typical Tensile Properties
Condition |
Elongation |
Tensile Strength |
Yield Strength |
As Welded |
37 % |
85 ksi |
65 ksi |
Typical Weld Metal Analysis %
weld metal analysis |
Mn |
Mo |
Cu |
C |
Si |
Ferrite |
Ni |
Cr |
1.80 % |
0.30 % |
0.10 % |
0.03 % |
0.45 % |
9 FN % |
13.50 % |
23.50 % |
Approvals: |
CWB CSA W48; E309L-16 |
Classifications: |
ASME II SFA A5.4; ASME IX F No. 5; AWS A5.4; E309L-16/E309-16 |
Approvals are based on factory location. Please contact ESAB for more information.